Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.6 g/cm³ Show Material materials with Dichte of 8.6 g/cm³ |
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 825 - 990 °C Show Material materials with Schmelzpunkt of 825 - 990 °C | |
Wärmeleitfähigkeit | 23.0 °C | 55 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 55 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 5.00E+6 - 6.00E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 5.00E+6 - 6.00E+6 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | Rest Cu, total 0.4 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Phosphor | 0.01 - 0.35 % Show Material materials with Phosphor of 0.01 - 0.35 % |
Zink | 0.1 % Show Material materials with Zink of 0.1 % |
Zinn | 11 - 13 % Show Material materials with Zinn of 11 - 13 % |