Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Schmelzpunkt | 1070 - 1080 °C Show Material materials with Schmelzpunkt of 1070 - 1080 °C | ||
Spezifische Wärmekapazität | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Wärmeleitfähigkeit | 23.0 °C | 220 - 315 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 220 - 315 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 3.00E+7 - 4.50E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 3.00E+7 - 4.50E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | Cu+Ag > 99.5, total 0.1, for gas welding as G-CuAg with P > 0.02%, for inert gas welding P < 0.02% |
Arsen | 0.05 % Show Material materials with Arsen of 0.05 % |
Blei | 0.01 % Show Material materials with Blei of 0.01 % |
Eisen | 0.05 % Show Material materials with Eisen of 0.05 % |
Kupfer | 99.5 % Show Material materials with Kupfer of 99.5 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Phosphor | 0.01 - 0.05 % Show Material materials with Phosphor of 0.01 - 0.05 % |
Silber | 0.8 - 1.2 % Show Material materials with Silber of 0.8 - 1.2 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |