Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.4 g/cm³ Show Material materials with Dichte of 7.4 g/cm³ |
Thermisch
Property | Temperature | Value |
---|---|---|
Schmelzpunkt | 945 - 985 °C Show Material materials with Schmelzpunkt of 945 - 985 °C | |
Wärmeleitfähigkeit | 23.0 °C | 30 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 30 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 3.00E+6 - 5.00E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 3.00E+6 - 5.00E+6 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 6.5 - 8.5 % Show Material materials with Aluminium of 6.5 - 8.5 % |
Andere | Rest Cu, total 0.4 |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 1.5 - 3 % Show Material materials with Eisen of 1.5 - 3 % |
Mangan | 11 - 14 % Show Material materials with Mangan of 11 - 14 % |
Nickel | 1.5 - 3 % Show Material materials with Nickel of 1.5 - 3 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 0.15 % Show Material materials with Zink of 0.15 % |