Chemical properties
Property | Value |
---|---|
Aluminium | 8 - 10 % Show Material materials with Aluminium of 8 - 10 % |
Andere | Rest Cu, total 1.7 |
Eisen | 2 - 4 % Show Material materials with Eisen of 2 - 4 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 1 % Show Material materials with Zink of 1 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |