Chemical properties
Property | Value |
---|---|
Aluminium | 0.1 % Show Material materials with Aluminium of 0.1 % |
Andere | Rest Cu, total 0.6 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Magnesium | 0.05 % Show Material materials with Magnesium of 0.05 % |
Mangan | 1.5 - 3 % Show Material materials with Mangan of 1.5 - 3 % |
Nickel | 29 - 33 % Show Material materials with Nickel of 29 - 33 % |
Silizium | 0.05 % Show Material materials with Silizium of 0.05 % |
Zink | 0.1 % Show Material materials with Zink of 0.1 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |