Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | total 1.0 |
Bismut | 0.01 % Show Material materials with Bismut of 0.01 % |
Blei | 0.2 % Show Material materials with Blei of 0.2 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Phosphor | 0.05 - 0.1 % Show Material materials with Phosphor of 0.05 - 0.1 % |
Zink | 0.3 % Show Material materials with Zink of 0.3 % |
Zinn | 4 - 6 % Show Material materials with Zinn of 4 - 6 % |