Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Andere | total 1.0 |
Antimon | 0.5 % Show Material materials with Antimon of 0.5 % |
Blei | 2 - 4 % Show Material materials with Blei of 2 - 4 % |
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Zink | 5 - 7 % Show Material materials with Zink of 5 - 7 % |