Chemical properties
Property | Value |
---|---|
Aluminium | 9.5 - 11 % Show Material materials with Aluminium of 9.5 - 11 % |
Andere | Rest Cu, total 1.5 |
Antimon | 0.05 % Show Material materials with Antimon of 0.05 % |
Arsen | 0.05 % Show Material materials with Arsen of 0.05 % |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 3.5 - 5.5 % Show Material materials with Eisen of 3.5 - 5.5 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 3.5 - 5.5 % Show Material materials with Nickel of 3.5 - 5.5 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |