Chemical properties
Property | Value |
---|---|
Aluminium | 9 - 10.5 % Show Material materials with Aluminium of 9 - 10.5 % |
Andere | total 1.5 |
Blei | 0.1 % Show Material materials with Blei of 0.1 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Mangan | 1 - 2 % Show Material materials with Mangan of 1 - 2 % |
Nickel | 2 - 3 % Show Material materials with Nickel of 2 - 3 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |