Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Andere | total 1.2 |
Arsen | 0.05 % Show Material materials with Arsen of 0.05 % |
Blei | 20 - 26 % Show Material materials with Blei of 20 - 26 % |
Eisen | 0.6 % Show Material materials with Eisen of 0.6 % |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % |
Phosphor | 0.07 % Show Material materials with Phosphor of 0.07 % |