Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Andere | total 1.2 |
Antimon | 0.3 % Show Material materials with Antimon of 0.3 % |
Eisen | 0.6 % Show Material materials with Eisen of 0.6 % |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Zink | 0.1 % Show Material materials with Zink of 0.1 % |
Zinn | 2 - 3.5 % Show Material materials with Zinn of 2 - 3.5 % |