Chemical properties
Property | Value |
---|---|
Andere | total 0.5 |
Blei | 27 - 33 % Show Material materials with Blei of 27 - 33 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Nickel | 0.1 % Show Material materials with Nickel of 0.1 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Silber | 1.4 - 1.7 % Show Material materials with Silber of 1.4 - 1.7 % |
Zink | 0.1 % Show Material materials with Zink of 0.1 % |
Zinn | 0.1 - 0.7 % Show Material materials with Zinn of 0.1 - 0.7 % |