Chemical properties
Property | Value |
---|---|
Andere | total 0.7 |
Blei | 27 - 33 % Show Material materials with Blei of 27 - 33 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Nickel | 0.1 % Show Material materials with Nickel of 0.1 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Silber | 2.75 - 3.25 % Show Material materials with Silber of 2.75 - 3.25 % |
Zink | 0.1 % Show Material materials with Zink of 0.1 % |
Zinn | 0.3 % Show Material materials with Zinn of 0.3 % |