Chemical properties
Property | Value |
---|---|
Aluminium | 4.5 - 6 % Show Material materials with Aluminium of 4.5 - 6 % |
Andere | Rest Zn, total 2.0 |
Antimon | 0.1 % Show Material materials with Antimon of 0.1 % |
Blei | 1 % Show Material materials with Blei of 1 % |
Eisen | 2 - 4 % Show Material materials with Eisen of 2 - 4 % |
Kupfer | 63 - 68 % Show Material materials with Kupfer of 63 - 68 % |
Mangan | 1.5 - 2.5 % Show Material materials with Mangan of 1.5 - 2.5 % |
Zinn | 1 % Show Material materials with Zinn of 1 % |