Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Andere | Rest Zn, total 4.0 |
Blei | 2 % Show Material materials with Blei of 2 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kupfer | 57 - 62 % Show Material materials with Kupfer of 57 - 62 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Zinn | 1 % Show Material materials with Zinn of 1 % |