Chemical properties
Property | Value |
---|---|
Aluminium | 0.7 - 1.5 % Show Material materials with Aluminium of 0.7 - 1.5 % |
Andere | Rest Zn, total 0.7 |
Antimon | 0.1 % Show Material materials with Antimon of 0.1 % |
Blei | 0.4 % Show Material materials with Blei of 0.4 % |
Eisen | 0.75 - 1.5 % Show Material materials with Eisen of 0.75 - 1.5 % |
Kupfer | 57 - 61 % Show Material materials with Kupfer of 57 - 61 % |
Mangan | 0.1 - 0.6 % Show Material materials with Mangan of 0.1 - 0.6 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Zinn | 0.2 - 0.7 % Show Material materials with Zinn of 0.2 - 0.7 % |