Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 - 2 % Show Material materials with Aluminium of 0.5 - 2 % |
Andere | Rest Zn, total 5.0 |
Blei | 1.5 % Show Material materials with Blei of 1.5 % |
Eisen | 1 % Show Material materials with Eisen of 1 % |
Kupfer | 56 - 60 % Show Material materials with Kupfer of 56 - 60 % |
Mangan | 0.5 - 2 % Show Material materials with Mangan of 0.5 - 2 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Zinn | 1.5 % Show Material materials with Zinn of 1.5 % |