Chemical properties
Property | Value |
---|---|
Aluminium | 0.3 - 0.5 % Show Material materials with Aluminium of 0.3 - 0.5 % |
Andere | Rest Zn |
Blei | 1.5 - 2.5 % Show Material materials with Blei of 1.5 - 2.5 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kupfer | 58 - 61 % Show Material materials with Kupfer of 58 - 61 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zinn | 1 % Show Material materials with Zinn of 1 % |