Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Antimon | 0.3 % Show Material materials with Antimon of 0.3 % |
Blei | 1 - 1.5 % Show Material materials with Blei of 1 - 1.5 % |
Eisen | 0.2 - 0.25 % Show Material materials with Eisen of 0.2 - 0.25 % |
Kupfer | 86 - 89 % Show Material materials with Kupfer of 86 - 89 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Nickel | 2 % Show Material materials with Nickel of 2 % |
Phosphor | 0.03 - 0.05 % Show Material materials with Phosphor of 0.03 - 0.05 % |
Schwefel | 0.1 % Show Material materials with Schwefel of 0.1 % |
Silizium | 0.01 % Show Material materials with Silizium of 0.01 % |
Zink | 1 - 3 % Show Material materials with Zink of 1 - 3 % |
Zinn | 9 - 11 % Show Material materials with Zinn of 9 - 11 % |