Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.75 - 2.8 g/cm³ Show Material materials with Dichte of 2.75 - 2.8 g/cm³ | Typical for Cast 2xx.x Series Aluminium |
Mechanisch
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.9e-05 - 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.9e-05 - 2.3e-05 1/K | Typical for Cast 2xx.x Series Aluminium |
Schmelzpunkt | 510.0 - 790.0 °C Show Material materials with Schmelzpunkt of 510.0 - 790.0 °C | Typical for Cast 2xx.x Series Aluminium |
Spezifische Wärmekapazität | 875.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 875.0 - 963.0 J/(kg·K) | Typical for Cast 2xx.x Series Aluminium |
Wärmeleitfähigkeit | 120.0 - 150.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 120.0 - 150.0 W/(m·K) | Typical for Cast 2xx.x Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 16000000.0 - 23000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 16000000.0 - 23000000.0 S/m | Typical for Cast 2xx.x Series Aluminium |
spezifischer Widerstand | 4.347826086956522e-08 - 6.25e-08 Ω·m Show Material materials with spezifischer Widerstand of 4.347826086956522e-08 - 6.25e-08 Ω·m | Typical for Cast 2xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Eisen | 0.40 % Show Material materials with Eisen of 0.40 % | Pink Sheets | Casting |
Kupfer | 7.0 - 9.0 % Show Material materials with Kupfer of 7.0 - 9.0 % | Pink Sheets | Casting |
Magnesium | 5.6 - 6.5 % Show Material materials with Magnesium of 5.6 - 6.5 % | Pink Sheets | Casting |
Mangan | 0.3 - 0.7 % Show Material materials with Mangan of 0.3 - 0.7 % | Pink Sheets | Casting |
Nickel | 0.3 - 0.7 % Show Material materials with Nickel of 0.3 - 0.7 % | Pink Sheets | Casting |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | Pink Sheets | Casting |
Titan | 0.2 % Show Material materials with Titan of 0.2 % | Pink Sheets | Casting |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | Pink Sheets | Casting |