Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.65 - 2.7 g/cm³ Show Material materials with Dichte of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastizitätsmodul | 73.0 - 80.0 GPa Show Material materials with Elastizitätsmodul of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Härte, Brinell | 65.0 [-] Show Material materials with Härte, Brinell of 65.0 [-] | T51 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
75.0 [-] Show Material materials with Härte, Brinell of 75.0 [-] | T51 | Pink Sheets, ASTM B108 | Casting | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |||
Schubmodule | 2.8 GPa Show Material materials with Schubmodule of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Zugfestigkeit | 170.0 MPa Show Material materials with Zugfestigkeit of 170.0 MPa | T51 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
185.0 MPa Show Material materials with Zugfestigkeit of 185.0 MPa | T51 | Pink Sheets, ASTM B108 | Casting |
Thermisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 2.3e-05 1/K | Typical for Cast 3xx.x Series Aluminium | |||
Schmelzpunkt | 546.0 - 621.0 °C Show Material materials with Schmelzpunkt of 546.0 - 621.0 °C | T51 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting | |
Spezifische Wärmekapazität | 960.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium | |||
Wärmeleitfähigkeit | 130.0 - 180.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 - 180.0 W/(m·K) | Typical for Cast 3xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % | T51 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Eisen | 0.60 % Show Material materials with Eisen of 0.60 % | T51 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Kupfer | 1.0 - 1.5 % Show Material materials with Kupfer of 1.0 - 1.5 % | T51 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Magnesium | 0.4 - 0.6 % Show Material materials with Magnesium of 0.4 - 0.6 % | T51 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % | T51 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Silizium | 4.5 - 5.5 % Show Material materials with Silizium of 4.5 - 5.5 % | T51 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Titan | 0.25 % Show Material materials with Titan of 0.25 % | T51 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Zink | 0.35 % Show Material materials with Zink of 0.35 % | T51 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |