Property | Value | Comment |
---|---|---|
Dichte | 2.65 - 2.7 g/cm³ Show Material materials with Dichte of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Bending Fatigue Strength | 140.0 MPa Show Material materials with Bending Fatigue Strength of 140.0 MPa | F | Pink Sheets, ASTM B85 | Casting | |
Elastizitätsmodul | 73.0 - 80.0 GPa Show Material materials with Elastizitätsmodul of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |||
Schubmodule | 2.8 GPa Show Material materials with Schubmodule of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Zugfestigkeit | 305.0 MPa Show Material materials with Zugfestigkeit of 305.0 MPa | F | Pink Sheets, ASTM B85 | Casting |
Thermisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 2.3e-05 1/K | Typical for Cast 3xx.x Series Aluminium | |||
Schmelzpunkt | 557.0 - 596.0 °C Show Material materials with Schmelzpunkt of 557.0 - 596.0 °C | F | Pink Sheets, ASTM B85 | Casting | |
Spezifische Wärmekapazität | 960.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium | |||
Wärmeleitfähigkeit | 130.0 - 180.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 - 180.0 W/(m·K) | Typical for Cast 3xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Eisen | 2.00 % Show Material materials with Eisen of 2.00 % | F | Pink Sheets, ASTM B85 | Casting |
Kupfer | 0.6 % Show Material materials with Kupfer of 0.6 % | F | Pink Sheets, ASTM B85 | Casting |
Magnesium | 0.4 - 0.6 % Show Material materials with Magnesium of 0.4 - 0.6 % | F | Pink Sheets, ASTM B85 | Casting |
Mangan | 0.35 % Show Material materials with Mangan of 0.35 % | F | Pink Sheets, ASTM B85 | Casting |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % | F | Pink Sheets, ASTM B85 | Casting |
Silizium | 9.0 - 10.0 % Show Material materials with Silizium of 9.0 - 10.0 % | F | Pink Sheets, ASTM B85 | Casting |
Zink | 0.5 % Show Material materials with Zink of 0.5 % | F | Pink Sheets, ASTM B85 | Casting |
Zinn | 0.15 % Show Material materials with Zinn of 0.15 % | F | Pink Sheets, ASTM B85 | Casting |