Chemical properties
Property | Value |
---|---|
Aluminium | 8 - 10 % Show Material materials with Aluminium of 8 - 10 % |
Blei | 0.1 % Show Material materials with Blei of 0.1 % |
Eisen | 1 - 4 % Show Material materials with Eisen of 1 - 4 % |
Kupfer | 85 - 90 % Show Material materials with Kupfer of 85 - 90 % |
Mangan | 0.1 - 1 % Show Material materials with Mangan of 0.1 - 1 % |
Nickel | 0.1 - 1 % Show Material materials with Nickel of 0.1 - 1 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |