Chemical properties
Property | Value |
---|---|
Aluminium | 8 - 10.5 % Show Material materials with Aluminium of 8 - 10.5 % |
Blei | 0.1 % Show Material materials with Blei of 0.1 % |
Eisen | 2.5 - 5 % Show Material materials with Eisen of 2.5 - 5 % |
Kupfer | 80 - 88 % Show Material materials with Kupfer of 80 - 88 % |
Mangan | 0.1 - 1.5 % Show Material materials with Mangan of 0.1 - 1.5 % |
Nickel | 1 - 3 % Show Material materials with Nickel of 1 - 3 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |