Chemical properties
Property | Value | Related Standards |
---|---|---|
Beryllium | 4.5 - 6.0 % Show Material materials with Beryllium of 4.5 - 6.0 % | Gold Sheets |
Chrom | 0.02 % Show Material materials with Chrom of 0.02 % | Gold Sheets |
Eisen | 0.40 % Show Material materials with Eisen of 0.40 % | Gold Sheets |
Kupfer | 0.05 % Show Material materials with Kupfer of 0.05 % | Gold Sheets |
Magnesium | 0.5 % Show Material materials with Magnesium of 0.5 % | Gold Sheets |
Mangan | 0.02 % Show Material materials with Mangan of 0.02 % | Gold Sheets |
Nickel | 0.02 % Show Material materials with Nickel of 0.02 % | Gold Sheets |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % | Gold Sheets |
Titan | 0.02 % Show Material materials with Titan of 0.02 % | Gold Sheets |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | Gold Sheets |