Chemical properties
Property | Value | Related Standards |
---|---|---|
Bor | 0.15 - 0.25 % Show Material materials with Bor of 0.15 - 0.25 % | Gold Sheets |
Eisen | 0.30 % Show Material materials with Eisen of 0.30 % | Gold Sheets |
Kalzium | 0.02 % Show Material materials with Kalzium of 0.02 % | Gold Sheets |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % | Gold Sheets |
Strontium | 9.0 - 11.0 % Show Material materials with Strontium of 9.0 - 11.0 % | Gold Sheets |
Titan | 0.9 - 1.2 % Show Material materials with Titan of 0.9 - 1.2 % | Gold Sheets |