Chemical properties
Property | Value |
---|---|
Aluminium | 6 - 9 % Show Material materials with Aluminium of 6 - 9 % |
Blei | 0.1 % Show Material materials with Blei of 0.1 % |
Eisen | 2 - 5 % Show Material materials with Eisen of 2 - 5 % |
Kupfer | 71 - 84 % Show Material materials with Kupfer of 71 - 84 % |
Mangan | 7 - 15 % Show Material materials with Mangan of 7 - 15 % |
Nickel | 1 - 4 % Show Material materials with Nickel of 1 - 4 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |