Chemical properties
Property | Value |
---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % |
Antimon | 0.2 % Show Material materials with Antimon of 0.2 % |
Blei | 1 % Show Material materials with Blei of 1 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kupfer | 86.5 - 89.5 % Show Material materials with Kupfer of 86.5 - 89.5 % |
Nickel | 0.8 % Show Material materials with Nickel of 0.8 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Silizium | 5E-3 % Show Material materials with Silizium of 5E-3 % |
Zink | 1 - 3 % Show Material materials with Zink of 1 - 3 % |
Zinn | 9 - 11 % Show Material materials with Zinn of 9 - 11 % |