Chemical properties
Property | Value |
---|---|
Aluminium | 8 - 10 % Show Material materials with Aluminium of 8 - 10 % |
Andere | Rest Cu, total 1.5 |
Blei | 0.03 % Show Material materials with Blei of 0.03 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Mangan | 1.5 - 2.5 % Show Material materials with Mangan of 1.5 - 2.5 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 1 % Show Material materials with Zink of 1 % |