Chemical properties
Property | Value |
---|---|
Aluminium | 0.15 % Show Material materials with Aluminium of 0.15 % |
Andere | Rest Cu, total 0.5 |
Beryllium | 1.85 - 2.1 % Show Material materials with Beryllium of 1.85 - 2.1 % |
Blei | 5E-3 % Show Material materials with Blei of 5E-3 % |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % |
Nickel | 0.2 - 0.4 % Show Material materials with Nickel of 0.2 - 0.4 % |
Silizium | 0.15 % Show Material materials with Silizium of 0.15 % |
Titan | 0.1 - 0.25 % Show Material materials with Titan of 0.1 - 0.25 % |