Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.9 |
Antimon | 0.3 % Show Material materials with Antimon of 0.3 % |
Arsen | 0.1 % Show Material materials with Arsen of 0.1 % |
Blei | 27 - 31 % Show Material materials with Blei of 27 - 31 % |
Eisen | 0.25 % Show Material materials with Eisen of 0.25 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Phosphor | 0.1 % Show Material materials with Phosphor of 0.1 % |
Silizium | 0.02 % Show Material materials with Silizium of 0.02 % |
Zink | 0.1 % Show Material materials with Zink of 0.1 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |