Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Andere | Rest Cu, total 0.9 |
Antimon | 3 - 4 % Show Material materials with Antimon of 3 - 4 % |
Arsen | 0.1 % Show Material materials with Arsen of 0.1 % |
Bismut | 0.025 % Show Material materials with Bismut of 0.025 % |
Blei | 18 - 22 % Show Material materials with Blei of 18 - 22 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Nickel | 3 - 4 % Show Material materials with Nickel of 3 - 4 % |
Phosphor | 0.15 - 0.3 % Show Material materials with Phosphor of 0.15 - 0.3 % |
Silizium | 0.02 % Show Material materials with Silizium of 0.02 % |
Zink | 3 - 4 % Show Material materials with Zink of 3 - 4 % |
Zinn | 0.5 % Show Material materials with Zinn of 0.5 % |