Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.4 - 8.9 g/cm³ Show Material materials with Dichte of 8.4 - 8.9 g/cm³ | Typical for Wrought Copper Nickel Silver Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 120 - 140 GPa Show Material materials with Elastizitätsmodul of 120 - 140 GPa | Typical for Wrought Copper Nickel Silver Grade |
Poissonzahl | 23.0 °C | 0.32 [-] Show Material materials with Poissonzahl of 0.32 [-] | Typical for Wrought Copper Nickel Silver Grade |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.9E-5 1/K | Typical for Wrought Copper Nickel Silver Grade |
Schmelzpunkt | 875 - 1135 °C Show Material materials with Schmelzpunkt of 875 - 1135 °C | Typical for Wrought Copper Nickel Silver Grade | |
Spezifische Wärmekapazität | 23.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) | Typical for Wrought Copper Nickel Silver Grade |
Wärmeleitfähigkeit | 23.0 °C | 21 - 116 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 - 116 W/(m·K) | Typical for Wrought Copper Nickel Silver Grade |
Chemical properties
Property | Value |
---|---|
Andere | Rest Zn, total 0.9 |
Antimon | 2E-3 % Show Material materials with Antimon of 2E-3 % |
Arsen | 0.01 % Show Material materials with Arsen of 0.01 % |
Bismut | 2E-3 % Show Material materials with Bismut of 2E-3 % |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Kupfer | 62 - 65 % Show Material materials with Kupfer of 62 - 65 % |
Magnesium | 0.05 % Show Material materials with Magnesium of 0.05 % |
Mangan | 0.3 % Show Material materials with Mangan of 0.3 % |
Nickel | 13.5 - 16.5 % Show Material materials with Nickel of 13.5 - 16.5 % |
Phosphor | 5E-3 % Show Material materials with Phosphor of 5E-3 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.15 % Show Material materials with Silizium of 0.15 % |