Mechanisch
Chemical properties
Property | Value |
---|---|
Aluminium | 8.5 - 11 % Show Material materials with Aluminium of 8.5 - 11 % |
Eisen | 3 - 5 % Show Material materials with Eisen of 3 - 5 % |
Kupfer | 81 - 88 % Show Material materials with Kupfer of 81 - 88 % |
Mangan | 0.5 - 2 % Show Material materials with Mangan of 0.5 - 2 % |
Nickel | 0.5 - 2 % Show Material materials with Nickel of 0.5 - 2 % |