Mechanisch
Chemical properties
Property | Value |
---|---|
Aluminium | 9 - 12 % Show Material materials with Aluminium of 9 - 12 % |
Eisen | 3 - 5 % Show Material materials with Eisen of 3 - 5 % |
Kupfer | 80 - 87 % Show Material materials with Kupfer of 80 - 87 % |
Mangan | 0.5 - 2 % Show Material materials with Mangan of 0.5 - 2 % |
Nickel | 0.5 - 2 % Show Material materials with Nickel of 0.5 - 2 % |