Chemical properties
Property | Value |
---|---|
Aluminium | 2.5 - 5 % Show Material materials with Aluminium of 2.5 - 5 % |
Andere | Rest Zn |
Blei | 0.2 % Show Material materials with Blei of 0.2 % |
Eisen | 1.5 - 4 % Show Material materials with Eisen of 1.5 - 4 % |
Kupfer | 60 - 66 % Show Material materials with Kupfer of 60 - 66 % |
Mangan | 1.5 - 4 % Show Material materials with Mangan of 1.5 - 4 % |
Nickel | 3 % Show Material materials with Nickel of 3 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |