Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Antimon | 0.2 % Show Material materials with Antimon of 0.2 % |
Blei | 0.8 % Show Material materials with Blei of 0.8 % |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % |
Kupfer | 85.5 - 88.3 % Show Material materials with Kupfer of 85.5 - 88.3 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Nickel | 1.8 % Show Material materials with Nickel of 1.8 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % |
Silizium | 0.01 % Show Material materials with Silizium of 0.01 % |
Zink | 2 % Show Material materials with Zink of 2 % |
Zinn | 10.7 - 13 % Show Material materials with Zinn of 10.7 - 13 % |