Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.7 - 8.7 g/cm³ Show Material materials with Dichte of 7.7 - 8.7 g/cm³ | Typical for Leaded Phosphor Bronze |
Mechanisch
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Spezifische Wärmekapazität | 23.0 °C | 380 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Andere | Rest Cu+Ag |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Chrom | 0.01 - 0.12 % Show Material materials with Chrom of 0.01 - 0.12 % |
Silizium | 2.7 - 3.4 % Show Material materials with Silizium of 2.7 - 3.4 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 1.2 - 1.9 % Show Material materials with Zinn of 1.2 - 1.9 % |