Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 8.47 g/cm³ Show Material materials with Dichte of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elastizitätsmodul | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass | ||
Poissonzahl | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass | ||
Zugfestigkeit | 621 MPa Show Material materials with Zugfestigkeit of 621 MPa | ASTM B505, ASTM B584 | Casting |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.5e-05 - 1.9e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5e-05 - 1.9e-05 1/K | Typical for Cast Copper Brass Yellow Brass |
Schmelzpunkt | 905 - 932 °C Show Material materials with Schmelzpunkt of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass |
Spezifische Wärmekapazität | 335 - 390 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Wärmeleitfähigkeit | 116 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 3 - 4.9 % Show Material materials with Aluminium of 3 - 4.9 % | ASTM B30, ASTM B505, ASTM B584 | Casting |
Blei | 0.1 % Show Material materials with Blei of 0.1 % | ASTM B30 | |
0.2 % Show Material materials with Blei of 0.2 % | ASTM B505, ASTM B584 | Casting | |
Eisen | 2 - 4 % Show Material materials with Eisen of 2 - 4 % | ASTM B30, ASTM B505, ASTM B584 | Casting |
Kupfer | 60 - 66 % Show Material materials with Kupfer of 60 - 66 % | ASTM B30, ASTM B505, ASTM B584 | Casting |
Mangan | 2.5 - 5 % Show Material materials with Mangan of 2.5 - 5 % | ASTM B30, ASTM B505, ASTM B584 | Casting |
Nickel | 0.8 % Show Material materials with Nickel of 0.8 % | ASTM B30 | |
1 % Show Material materials with Nickel of 1 % | ASTM B505, ASTM B584 | Casting | |
Zink | 22 - 28 % Show Material materials with Zink of 22 - 28 % | ASTM B30, ASTM B505, ASTM B584 | Casting |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % | ASTM B30 | |
0.2 % Show Material materials with Zinn of 0.2 % | ASTM B505, ASTM B584 | Casting |