Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elastizitätsmodul | 96 - 120 GPa Show Material materials with Elastizitätsmodul of 96 - 120 GPa | Typical for Cast Copper Bronze | ||
Poissonzahl | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Bronze | ||
Zugfestigkeit | 252 MPa Show Material materials with Zugfestigkeit of 252 MPa | ASTM B505 | Casting |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 1.9e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Schmelzpunkt | 760 - 1060 °C Show Material materials with Schmelzpunkt of 760 - 1060 °C | Typical for Cast Copper Bronze |
Spezifische Wärmekapazität | 376 - 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Wärmeleitfähigkeit | 12 - 81 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 0.005 % Show Material materials with Aluminium of 0.005 % | ASTM B30, ASTM B505 | Casting |
Antimon | 0.2 % Show Material materials with Antimon of 0.2 % | ASTM B30 | |
0.25 % Show Material materials with Antimon of 0.25 % | ASTM B505 | Casting | |
Blei | 1 - 2.3 % Show Material materials with Blei of 1 - 2.3 % | ASTM B30 | |
1 - 2.5 % Show Material materials with Blei of 1 - 2.5 % | ASTM B505 | Casting | |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % | ASTM B30 | |
0.15 % Show Material materials with Eisen of 0.15 % | ASTM B30 | ||
0.2 % Show Material materials with Eisen of 0.2 % | ASTM B505 | Casting | |
0.2 % Show Material materials with Eisen of 0.2 % | |||
Kupfer | 86 - 89 % Show Material materials with Kupfer of 86 - 89 % | ASTM B30, ASTM B505 | Casting |
Nickel | 0.8 % Show Material materials with Nickel of 0.8 % | ASTM B30 | |
1 % Show Material materials with Nickel of 1 % | ASTM B505 | Casting | |
Phosphor | 0.25 % Show Material materials with Phosphor of 0.25 % | ASTM B30 | |
0.3 % Show Material materials with Phosphor of 0.3 % | ASTM B30 | ||
1.5 % Show Material materials with Phosphor of 1.5 % | ASTM B505 | Casting | |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % | ASTM B30, ASTM B505 | Casting |
Silizium | 0.005 % Show Material materials with Silizium of 0.005 % | ASTM B30, ASTM B505 | Casting |
Zink | 0.7 % Show Material materials with Zink of 0.7 % | ASTM B505 | Casting |
0.8 % Show Material materials with Zink of 0.8 % | ASTM B30 | ||
Zinn | 9 - 11 % Show Material materials with Zinn of 9 - 11 % | ASTM B505 | Casting |
9.3 - 11 % Show Material materials with Zinn of 9.3 - 11 % | ASTM B30 |