Mechanisch
Property | Value | Comment |
---|---|---|
Elastizitätsmodul | 96 - 120 GPa Show Material materials with Elastizitätsmodul of 96 - 120 GPa | Typical for Cast Copper Bronze |
Poissonzahl | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Bronze |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 1.9e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Schmelzpunkt | 760 - 1060 °C Show Material materials with Schmelzpunkt of 760 - 1060 °C | Typical for Cast Copper Bronze |
Spezifische Wärmekapazität | 376 - 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Wärmeleitfähigkeit | 12 - 81 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Aluminium | 10.5 - 11.5 % Show Material materials with Aluminium of 10.5 - 11.5 % | ASTM B30, ASTM B271, ASTM B505 |
Blei | 0.03 % Show Material materials with Blei of 0.03 % | ASTM B30, ASTM B271, ASTM B505 |
Chrom | 0.05 % Show Material materials with Chrom of 0.05 % | ASTM B30 |
Eisen | 4 - 5.5 % Show Material materials with Eisen of 4 - 5.5 % | ASTM B30, ASTM B271, ASTM B505 |
Kobalt | 0.2 % Show Material materials with Kobalt of 0.2 % | ASTM B30 |
Kupfer | 74.5 % Show Material materials with Kupfer of 74.5 % | ASTM B30, ASTM B271, ASTM B505 |
Magnesium | 0.05 % Show Material materials with Magnesium of 0.05 % | ASTM B30 |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % | ASTM B30, ASTM B271, ASTM B505 |
Nickel | 4.2 - 6 % Show Material materials with Nickel of 4.2 - 6 % | ASTM B30, ASTM B271, ASTM B505 |
Silizium | 0.15 % Show Material materials with Silizium of 0.15 % | ASTM B30, ASTM B271, ASTM B505 |
Zink | 0.3 % Show Material materials with Zink of 0.3 % | ASTM B30, ASTM B271, ASTM B505 |
Zinn | 0.25 % Show Material materials with Zinn of 0.25 % | ASTM B30, ASTM B271, ASTM B505 |