Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 25 % Show Material materials with Dehnung A50 of 25 % | |
Elastizitätsmodul | 23.0 °C | 120 - 156 GPa Show Material materials with Elastizitätsmodul of 120 - 156 GPa | Typical for Cast Copper Nickel Grade |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Nickel Grade |
Streckgrenze Rp0,5 | 23.0 °C | 241 MPa Show Material materials with Streckgrenze Rp0,5 of 241 MPa | |
Zugfestigkeit | 23.0 °C | 448 MPa Show Material materials with Zugfestigkeit of 448 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | Typical for Cast Copper Nickel Grade |
Schmelzpunkt | 1100 - 1240 °C Show Material materials with Schmelzpunkt of 1100 - 1240 °C | Typical for Cast Copper Nickel Grade | |
Spezifische Wärmekapazität | 23.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) | Typical for Cast Copper Nickel Grade |
Wärmeleitfähigkeit | 23.0 °C | 23 - 45 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 23 - 45 W/(m·K) | Typical for Cast Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % |
Andere | Rest Cu |
Blei | 0.01 - 0.03 % Show Material materials with Blei of 0.01 - 0.03 % |
Eisen | 0.25 - 1.5 % Show Material materials with Eisen of 0.25 - 1.5 % |
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % |
Kupfer | 65 - 67 % Show Material materials with Kupfer of 65 - 67 % |
Mangan | 0.8 - 1.5 % Show Material materials with Mangan of 0.8 - 1.5 % |
Nickel | 28 - 32 % Show Material materials with Nickel of 28 - 32 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 0.3 - 0.5 % Show Material materials with Silizium of 0.3 - 0.5 % |