Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.4 - 8.9 g/cm³ Show Material materials with Dichte of 8.4 - 8.9 g/cm³ | Typical for Cast Copper Nickel Silver Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 10 % Show Material materials with Dehnung A50 of 10 % | |
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Cast Copper Nickel Silver Grade |
Poissonzahl | 23.0 °C | 0.32 [-] Show Material materials with Poissonzahl of 0.32 [-] | Typical for Cast Copper Nickel Silver Grade |
Streckgrenze Rp0,5 | 23.0 °C | 117 - 138 MPa Show Material materials with Streckgrenze Rp0,5 of 117 - 138 MPa | |
Zugfestigkeit | 23.0 °C | 276 MPa Show Material materials with Zugfestigkeit of 276 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 - 1.9E-5 1/K | Typical for Cast Copper Nickel Silver Grade |
Schmelzpunkt | 1010 - 1180 °C Show Material materials with Schmelzpunkt of 1010 - 1180 °C | Typical for Cast Copper Nickel Silver Grade | |
Spezifische Wärmekapazität | 23.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) | Typical for Cast Copper Nickel Silver Grade |
Wärmeleitfähigkeit | 23.0 °C | 22 - 29 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 22 - 29 W/(m·K) | Typical for Cast Copper Nickel Silver Grade |
Chemical properties
Property | Value |
---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % |
Antimon | 0.25 % Show Material materials with Antimon of 0.25 % |
Blei | 3 - 5 % Show Material materials with Blei of 3 - 5 % |
Eisen | 1 - 1.5 % Show Material materials with Eisen of 1 - 1.5 % |
Kupfer | 63 - 67 % Show Material materials with Kupfer of 63 - 67 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 19 - 21.5 % Show Material materials with Nickel of 19 - 21.5 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.08 % Show Material materials with Schwefel of 0.08 % |
Silizium | 0.05 - 0.15 % Show Material materials with Silizium of 0.05 - 0.15 % |
Zink | 3 - 9 % Show Material materials with Zink of 3 - 9 % |
Zinn | 3.5 - 4.5 % Show Material materials with Zinn of 3.5 - 4.5 % |