Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 - 2 % Show Material materials with Aluminium of 0.5 - 2 % |
Andere | Rest Cu |
Blei | 0.25 % Show Material materials with Blei of 0.25 % |
Eisen | 1 - 5.5 % Show Material materials with Eisen of 1 - 5.5 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 1 - 5.5 % Show Material materials with Nickel of 1 - 5.5 % |
Silizium | 0.5 - 2 % Show Material materials with Silizium of 0.5 - 2 % |
Zink | 0.5 - 5 % Show Material materials with Zink of 0.5 - 5 % |