Mechanisch
Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 - 2 % Show Material materials with Aluminium of 0.5 - 2 % |
Andere | Rest Cu |
Blei | 0.09 - 0.25 % Show Material materials with Blei of 0.09 - 0.25 % |
Eisen | 3 - 5.5 % Show Material materials with Eisen of 3 - 5.5 % |
Mangan | 0.2 - 0.5 % Show Material materials with Mangan of 0.2 - 0.5 % |
Nickel | 3.5 - 5.5 % Show Material materials with Nickel of 3.5 - 5.5 % |
Silizium | 0.5 - 2 % Show Material materials with Silizium of 0.5 - 2 % |
Zink | 0.5 - 2 % Show Material materials with Zink of 0.5 - 2 % |