Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 - 3 % Show Material materials with Aluminium of 0.5 - 3 % |
Blei | 2 % Show Material materials with Blei of 2 % |
Eisen | 1 % Show Material materials with Eisen of 1 % |
Kupfer | 54 % Show Material materials with Kupfer of 54 % |
Mangan | 11 - 15 % Show Material materials with Mangan of 11 - 15 % |
Nickel | 4 - 6 % Show Material materials with Nickel of 4 - 6 % |
Zink | 19 - 25 % Show Material materials with Zink of 19 - 25 % |
Zinn | 1 % Show Material materials with Zinn of 1 % |