Chemical properties
Property | Value |
---|---|
Aluminium | 0.25 - 3 % Show Material materials with Aluminium of 0.25 - 3 % |
Blei | 0.5 - 2.5 % Show Material materials with Blei of 0.5 - 2.5 % |
Eisen | 1 % Show Material materials with Eisen of 1 % |
Kupfer | 55 - 61 % Show Material materials with Kupfer of 55 - 61 % |
Mangan | 17 - 23 % Show Material materials with Mangan of 17 - 23 % |
Nickel | 5 % Show Material materials with Nickel of 5 % |
Zink | 17 - 23 % Show Material materials with Zink of 17 - 23 % |