Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Blei | 0.03 % Show Material materials with Blei of 0.03 % |
Eisen | 1.2 - 1.8 % Show Material materials with Eisen of 1.2 - 1.8 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Kupfer | 84.5 % Show Material materials with Kupfer of 84.5 % |
Mangan | 1.2 - 1.5 % Show Material materials with Mangan of 1.2 - 1.5 % |
Nickel | 9.2 - 11 % Show Material materials with Nickel of 9.2 - 11 % |
Niobium | 1 % Show Material materials with Niobium of 1 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |