Chemical properties
Property | Value |
---|---|
Aluminium | 8.8 - 10 % Show Material materials with Aluminium of 8.8 - 10 % |
Andere | Rest Cu, total 0.30 |
Blei | 0.03 % Show Material materials with Blei of 0.03 % |
Eisen | 4 - 5.5 % Show Material materials with Eisen of 4 - 5.5 % |
Magnesium | 0.05 % Show Material materials with Magnesium of 0.05 % |
Mangan | 3 % Show Material materials with Mangan of 3 % |
Nickel | 4 - 5.5 % Show Material materials with Nickel of 4 - 5.5 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |