Chemical properties
Property | Value |
---|---|
Aluminium | 8 - 11 % Show Material materials with Aluminium of 8 - 11 % |
Blei | 0.1 % Show Material materials with Blei of 0.1 % |
Eisen | 3.5 - 5.5 % Show Material materials with Eisen of 3.5 - 5.5 % |
Kupfer | 76 % Show Material materials with Kupfer of 76 % |
Mangan | 3 % Show Material materials with Mangan of 3 % |
Nickel | 3.5 - 6.5 % Show Material materials with Nickel of 3.5 - 6.5 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |